Enzyme-induced biodegradation of polycarbonate polyurethanes: Dependence on hard-segment concentration
Authors:
- 29 May 2001
- journal article
- research article
- Published by Wiley in Journal of Biomedical Materials Research
- Vol. 56 (4) , 516-528
Abstract
Polycarbonate-based polyurethanes with varying hard segment contents were synthesized. The physical and chemical structures were characterized by using gel permeation chromatography, differential scanning calorimetry, water uptake testing, Fourier transform infrared, and attenuated total reflectance–Fourier transform infrared. The polymers were incubated with cholesterol esterase in a phosphate buffer solution at 37°C over 10 weeks. A higher resistance to hydrolytic degradation was observed in polycarbonate-based urethanes with higher hard segment content. The analysis of the material structures revealed that the degradation of polycarbonate-based urethanes was preferentially initiated at non-hydrogen-bonded carbonates and urethanes. Although the crystallinity of the polycarbonate soft segment may contribute to reducing the hydrolytic degradation catalyzed by cholesterol esterase, it was found to be relatively minor in comparison to the importance of hydrogen bonding between the carbonate and urethane groups. These observations suggest that the biostability of polyurethanes and specifically polycarbonate-based polyurethanes can be improved by manipulating the degree of hydrogen bonding within the materials. © 2001 John Wiley & Sons, Inc. J Biomed Mater Res 56: 516–528, 2001Keywords
This publication has 33 references indexed in Scilit:
- Neutrophil-mediated degradation of segmented polyurethanesBiomaterials, 1995
- The enzymatic hydrolysis of a synthetic biomembrane: A new substrate for cholesterol and carboxyl esterasesJournal of Biomaterials Science, Polymer Edition, 1995
- Biodegradation evaluation of polyether and polyester‐urethanes with oxidative and hydrolytic enzymesJournal of Biomedical Materials Research, 1994
- Human plasma α2‐macroglobulin promotes in vitro oxidative stress cracking of pellethane 2363‐80A: In vivo and in vitro correlationsJournal of Biomedical Materials Research, 1993
- Enzyme–biomaterial interactions: Effect of biosystems on degradation of polyurethanesJournal of Biomedical Materials Research, 1993
- Effect of soft segment chemistry on the biostability of segmented polyurethanes. I. In vitro oxidationJournal of Biomedical Materials Research, 1991
- Analysis of in vitro enzymatic and oxidative degradation of polyurethanesJournal of Biomedical Materials Research, 1988
- Polyether Polyurethanes: Biostable or Not?Journal of Biomaterials Applications, 1988
- Biostability of Polyurethane Elastomers: A Critical ReviewJournal of Biomaterials Applications, 1988