Impact of Scaling Thickness on the Ferroelectric Properties of Pt/Al₀.₈Sc₀.₂N/Pt Capacitors

Authors:

Abstract
In this work, the effects of reducing the thickness of Al $_{\text{0.8}}$ Sc $_{\text{0.2}}$ N films from 100 to 40 nm on the ferroelectric properties of Pt/Al $_{\text{0.8}}$ Sc $_{\text{0.2}}$ N/Pt capacitors were investigated. As Al $_{\text{0.8}}$ Sc $_{\text{0.2}}$ N film thickness decreases, remanent polarization significantly drops, and coercive field ( $\textit{E}_{\text{c}}$ ) increases, which origins from the diminished c -axis orientation and reduced crystalline size. Piezoresponse force microscopy results confirm polarization switching in all films, with thinner films exhibiting larger $\textit{E}_{\text{c}}$ and lower initial polarization. Notably, the thinner films show the lower leakage current, attributed to a decrease in nitrogen vacancies. Moreover, thinner Al $_{\text{0.8}}$ Sc $_{\text{0.2}}$ N films exhibit better endurance performance, with a maximum switching cycle of 10 $^{\text{5}}$ cycles achieved for the 40-nm Al $_{\text{0.8}}$ Sc $_{\text{0.2}}$ N film. These results underscore the critical role of film thickness in optimizing aluminum scandium nitride (AlScN) thin films for high-performance ferroelectric applications, providing crucial insights for future device development.
Funding Information
  • China Postdoctoral Science Foundation (2023M742732)
  • Postdoctoral Fellowship Program of CPSF (GZC20241303)
  • National Natural Science Foundation of China (62025402, 62090033, 92364204, 9226420, 62293522)
  • Major Program of Zhejiang Natural Science Foundation (LDT23F04024F04)

This publication has 40 references indexed in Scilit: