Remineralization Potential of Three Restorative Glass Ionomer Cements: An In Vitro Study
Open Access
- 22 March 2023
- journal article
- research article
- Published by MDPI AG in Journal of Clinical Medicine
- Vol. 12 (6) , 2434
Abstract
The aim of this in vitro study was to evaluate the remineralizing ability of three glass ionomers on demineralized dentin with different thicknesses and time periods. Fifty third molars were obtained and were sectioned into 1-, 2-, and 3-mm thick slices (n = 36 for each thickness). The specimens were demineralized with 18% EDTA for 2 h. From the glass ionomer cements (GICs) under study (Ketac Molar Aplicap, Equia Forte, or Riva Light Cure), 1 mm was placed over each slice, set, and preserved in PBS until observation after 1, 7, 14, and 28 days after placement. For each material, thickness, and time, three samples were prepared. Using Fourier Transform Infrared Spectrometry (FTIR), apatite formation was determined on the side opposite to that on which the material had been placed. By means of Energy Dispersive Spectroscopy (EDX), the changes in the Calcium/Phosphate (Ca/P) ratio were evaluated. These changes were compared between the different materials by means of a two-way ANOVA test, considering time and dentin thickness, for a significance level of p < 0.05. Results: FTIR showed a peak at 1420 cm−1, evidencing the presence of carbonated hydroxyapatite in all the materials after 14 days, which indicates that a remineralization process occurred. Riva Light Cure showed the most homogeneous results at all depths at 28 days. The Ca/P ratio was maximum at 7 days in 2 mm of dentin for Riva Light Cure and Equia Forte HT (3.16 and 3.07; respectively) and for Ketac Molar at 14 days in 1 mm (3.67). All materials induced remineralization. Equia Forte achieved the greatest effect at 2 mm and Ketac Molar at 1 mm, whereas Riva Light Cure showed similar results at all depths. In terms of Ca/P ratio, Equia Forte and Riva Light Cure remineralized best at 2 mm, whereas for Ketac Molar, it was 1 mm. Carbonate apatite formation was higher at 24 h and 7 days for Ketac Molar, whereas it decreased at 14 days for Ketac Molar and peaked in Riva Light Cure and Equia Forte.Keywords
This publication has 34 references indexed in Scilit:
- Sealers and Warm Gutta-percha Obturation TechniquesJournal of Endodontics, 2015
- β‐Dicalcium silicate‐based cement: Synthesis, characterization and in vitro bioactivity and biocompatibility studiesJournal of Biomedical Materials Research Part A, 2013
- Polydopamine-Induced Tooth RemineralizationACS Applied Materials & Interfaces, 2012
- Biomimetic remineralization of human dentin using promising innovative calcium-silicate hybrid “smart” materialsDental Materials, 2011
- Can Caries-Affected Dentin be Completely Remine-ralized by Guided Tissue Remineralization?Dental Hypotheses, 2010
- Resin-modified Glass-ionomer Setting Reaction CompetitionJournal of Dental Research, 2009
- Biomechanical Perspective on the Remineralization of DentinCaries Research, 2009
- Effect of strontium in combination with fluoride on enamel remineralisation in vitroArchives of Oral Biology, 2008
- Fourier Transform Infrared Spectroscopic Study of the Role of Tartaric Acid in Glass-ionomer Dental CementsJournal of Dental Research, 1988
- Relationship between Hardness, Discoloration, and Microbial Invasion in Carious DentinJournal of Dental Research, 1966