Vacuum brazing of TZM alloy and graphite with Ti-35Ni alloy: Microstructure, properties, and mechanism

Authors:

Abstract
Reliable TZM/graphite brazed joint was obtained in a vacuum using Ti-35Ni alloy in the present work. The interfacial microstructure, shear strength, and fracture characteristics of the brazed joints were all analyzed. In addition, the formation mechanism of the brazed joint was investigated in detail. The typical interfacial microstructure of the TZM/graphite joint brazed at 1200°C for 10 min was TZM/Ti(s,s)/TiNi+Ti2Ni/TiC/graphite. The width of the brazing seam increased and then decreased with the elevated temperature, while the thickness of the TiC layer gradually increased. In addition, the amount of Ti2Ni phase in the brazing seam decreased above 1200°C and eventually disappeared at 1220°C. An optimal shear strength of 14.5 MPa was achieved for the TZM/graphite joint at a brazing temperature of 1300°C for 10 min. At the optimum brazing temperature, the fracture path of the joint started in the TiC layer and then extended to the interior of the graphite substrate.

This publication has 25 references indexed in Scilit: