Abstract
A cubic δ-TaNδ-TaN thin film with an electrical resistivity of 400μΩcm400μΩcm was successfully obtained by suppressing the formation of Ta3N5Ta3N5 using two-step atomic layer deposition independent of NH3NH3 dosage. The deposition cycle involved two chemical reaction steps: The formation of elemental tantalum (Ta) by reducing tantalum pentafluoride (TaF5)(TaF5) with hydrogen plasma and the subsequent nitridation of the preformed Ta with NH3NH3 at 200–350°C200–350°C . The microstructure of the preformed Ta was β-Taβ-Ta phase with an electrical resistivity of 220μΩcm220μΩcm , which was formed without regard to the deposition temperature. At a deposition temperature of less than 250°C250°C , cubic δ-TaNδ-TaN with a Ta∕NTa∕N ratio of 1 was achieved independent of the NH3NH3 dosage. However, at a deposition temperature of greater than 300°C300°C , the resistivity of Ta–N-based thin film increased abruptly as the NH3NH3 dosage exceeded 16.08×1019molecules∕cm316.08×1019molecules∕cm3 due to the formation of Ta3N5Ta3N5 .

This publication has 14 references indexed in Scilit: