Abstract
Y 2 Si 2 O 7 coatings were formed on Hi‐Nicalon‐S SiC fibers by reaction of solution‐derived YPO 4 coatings with glass SiO 2 scales formed by fiber oxidation. Two oxidation methods were used: pre‐oxidation, where fibers were oxidized prior to YPO 4 coating, or post‐oxidation, where fibers were first coated with YPO 4 and then oxidized. Fibers with YPO 4 /SiO 2 films were heat‐treated in argon at 1200°C for 20 hours to react YPO 4 and SiO 2 to Y 2 Si 2 O 7 . The effects of SiO 2 to YPO 4 film thicknesses on fiber strength and on the Y 2 Si 2 O 7 formation kinetics were investigated. An optimized process to obtain single‐phase continuous Y 2 Si 2 O 7 coatings on Hi‐Nicalon‐S fibers with low loss in fiber strength is suggested.
Funding Information
  • Air Force Research Laboratory (FA8650‐10‐D‐5226, FA8650‐15‐D‐5230)

This publication has 35 references indexed in Scilit: