Void swelling at low displacement rates in annealed 12X18HgT stainless steel at 4–56 dpa and 280–332 °C

Authors:
  • SPS.I. Porollo
    S.I. Porollo
  • YKYu.V. Konobeev
    Yu.V. Konobeev
  • ADA.M. Dvoriashin
    A.M. Dvoriashin
  • AVA.N. Vorobjev
    A.N. Vorobjev
  • VKV.M. Krigan
    V.M. Krigan

Abstract
No abstract available