Thermoelectric hysteresis in Nicrosil and Nisil
Author:
- 1 November 1987
- journal article
- Published by IOP Publishing in Journal of Physics E: Scientific Instruments
- Vol. 20 (11) , 1368-1373
Abstract
Hysteresis in the Seebeck coefficients of the thermocouple alloys Nicrosil and Nisil was studied over the temperature range, 200 to 1200 degrees C, for heating periods up to 300 h. The alloys were thermoelements in Nicrosil-sheathed mineral-insulated cable. For both alloys hysteresis peaks were found near 400 and 700 degrees C. In Nicrosil the lower temperature peak was small (-1) and the peak near 700 degrees C increased rapidly to about 0.3 mu V K-1) for 50 h of heating and changed little thereafter. Both peaks in Nisil were about 0.2 mu V K-1 in magnitude after 100 h of heating and increased steadily with time, reaching 0.3 mu V K-1 at 300 H. The study showed that hysteresis was the main cause of instability in such thermocouples and suggested that hysteresis in Nisil could be greatly reduced during manufacture.Keywords
This publication has 3 references indexed in Scilit:
- Ni-based thermocouples in the mineral-insulated metal-sheathed format: thermoelectric instabilities to 1100 degrees CJournal of Physics E: Scientific Instruments, 1986
- Temperature measurement errors with type K (Chromel vs Alumel) thermocouples due to short-ranged ordering in ChromelReview of Scientific Instruments, 1975
- Thermoelectric characteristics of binary alloys of nickelActa Metallurgica, 1966