Investigation of fracture causes of the titanium alloy drill pipe in ultra-short radius horizontal well drilling
Authors:
- Qiang LiuQLQiang Liu
- Ke TongKTKe Tong
- Guo-Chuan ZhuGZGuo-Chuan Zhu
- Yi TanYTYi Tan
- Juantao ZhangJZJuantao Zhang
- Xin XuXXXin Xu
- Xiaojun LiXLXiaojun Li
- Sheng-Yin SongSSSheng-Yin Song
- 15 June 2022
- journal article
- research article
- Published by Elsevier in Engineering Failure Analysis
- Vol. 140
Abstract
No abstract availableKeywords
Funding Information
- National Key Research and Development Program of China (2021YFB3700804)
- China National Petroleum Corporation (2021DJ2703)
- Natural Science Foundation of Shaanxi Province (2021JM-607)
This publication has 7 references indexed in Scilit:
- Fracture response of 1422-mm diameter pipe with double-V groove weld joints and circumferential crack in fusion lineEngineering Failure Analysis, 2020
- Microstructure, precipitate and property evolution in cold-rolled Ti-V high strength low alloy steelMaterials & Design, 2020
- A novel high-strength β-Ti alloy with hierarchical distribution of α-phase: The superior combination of strength and ductilityMaterials & Design, 2019
- Experimental and numerical study of drill string dynamics in gas drilling of horizontal wellsJournal of Natural Gas Science and Engineering, 2015
- Applying titanium alloys in drilling and offshore production systemsJOM, 2001
- Recent developments in titanium alloy application in the energy industryMaterials Science and Engineering: A, 1998
- Influence of processing on microstructure and mechanical properties of (α+β) titanium alloysMaterials Science and Engineering: A, 1998