Influence of Ceramic Thickness and Ceramic Materials on Fracture Resistance of Posterior Partial Coverage Restorations
Authors:
- 1 March 2015
- journal article
- Published by Operative Dentistry in Operative Dentistry
- Vol. 40 (2) , 211-217
Abstract
SUMMARY: This study evaluated the influence of ceramic thickness and ceramic materials on fracture resistance of posterior partial coverage ceramic restorations. Forty extracted molars were allocated into four groups (n=10) to test for two variables: 1) the thickness of ceramic (1 mm or 2 mm) and 2) the ceramic materials (a lithium disilicate glass-ceramic [IPS e.max] or leucite-reinforced glass ceramic [IPS Empress]). All ceramic restorations were luted with resin cement (Variolink II) on the prepared teeth. These luted specimens were loaded to failure in a universal testing machine, in the compression mode, with a crosshead speed of 1.0 mm/min. The data were analyzed using two-way analysis of variance and the Tukey Honestly Significantly Different multiple comparison test (α =0.05). The fracture resistance revealed a significant effect for materials (p<0.001); however, the thickness of ceramic was not significant (p=0.074), and the interaction between the thickness of ceramic and the materials was not significant (p=0.406). Mean (standard deviation) fracture resistance values were as follows: a 2-mm thickness of a lithium disilicate bonded to tooth structure (2505 [401] N) revealed a significantly higher fracture resistance than did a 1-mm thickness of leucite-reinforced (1569 [452] N) and a 2-mm thickness of leucite-reinforced ceramic bonded to tooth structure (1716 [436] N) (p<0.05). There was no significant difference in fracture resistance values between a lithium disilicate ceramic at 1-mm thickness (2105 [567] N) and at 2-mm thickness. Using a lithium disilicate glass ceramic for partial coverage restoration significantly improved fracture resistance compared to using a leucite-reinforced glass ceramic. The thickness of ceramic had no significant effect on fracture resistance when the ceramics were bonded to the underlying tooth structure.Keywords
This publication has 18 references indexed in Scilit:
- Ceramics as biomaterials for dental restorationExpert Review of Medical Devices, 2008
- The Effects of Tooth Preparation Cleansing Protocols on the Bond Strength of Self-adhesive Resin Luting Cement to Contaminated DentinOperative Dentistry, 2008
- Fracture behavior of lithia disilicate- and leucite-based ceramicsDental Materials, 2004
- Biaxial flexural strength, elastic moduli, and x-ray diffraction characterization of three pressable all-ceramic materialsThe Journal of Prosthetic Dentistry, 2003
- The effect of cement type and mixing on the bi-axial fracture strength of cemented aluminous core porcelain discsDental Materials, 2003
- Wear of composite resin veneering materials in a dual‐axis chewing simulatorJournal of Oral Rehabilitation, 1999
- Short‐Term Results of IPS‐Empress Inlays and OnlaysJournal of Prosthodontics, 1996
- Pulpal evaluation of teeth restored with fixed prosthesesThe Journal of Prosthetic Dentistry, 1992
- Relative flexural strength of dental restorative ceramicsDental Materials, 1990
- Limits of human bite strengthThe Journal of Prosthetic Dentistry, 1986