Abstract
Monolithic TiN and multilayered structures of TiN films that alternate with thin Ti interlayers were coated by filtered arc deposition onto a stainless steel substrate. Microscratch tests with a diamond indenter of 5-μm radius were carried out in combination with focused ion beam (FIB) sectioning and scanning and transmission electron microscopy to explore the controlling deformation mechanisms of these TiN coatings in relation to their microstructural design. It was found that for the monolithic TiN coating, columnar TiN grains slid against each other under normal forces and, at the same time, tilted under tangential forces. For the TiN multilayers, however, intercolumnar shear sliding was suppressed considerably by the multilayered structure and the interlayers, and grain tilting occurred largely within the upper TiN layer, presumably due to the shear effect of the soft Ti interlayers. With further increases in tangential force, rupture of TiN grains was observed within both types of coatings; for the TiN multilayers, rupture of TiN grains occurred predominantly within the layers close to the steel substrates. It can be concluded that the application of TiN multilayers provides better resistance to contact damage than the traditional monolithic TiN coatings did.Keywords
This publication has 16 references indexed in Scilit:
- Microstructural effects on indentation failure mechanisms in TiN coatings: Finite element simulationsActa Materialia, 2007
- Deposition of nanocomposite thin films by a hybrid cathodic arc and chemical vapour techniqueSurface and Coatings Technology, 2006
- Contact deformation of TiN coatings on metallic substratesMaterials Science and Engineering: A, 2006
- Deposition of nanocomposite TiN-Si3N4 thin films by hybrid cathodic arc and chemical vapor processApplied Physics A, 2005
- Nature of contact deformation of TiN films on steelJournal of Materials Research, 2004
- Mechanisms of coating failure as demonstrated by scratch and indentation testing of TiN coated HSSSurface Engineering, 2000
- Can scratch testing be used as a model for the abrasive wear of hard coatings?Wear, 1999
- Failure mode maps in the thin film scratch adhesion testTribology International, 1997
- Examination of mechanical properties and failure mechanisms of TiN and Ti−TiN multilayer coatingsSurface and Coatings Technology, 1995
- Thick Ti/TiN multilayered coatings for abrasive and erosive wear resistanceSurface and Coatings Technology, 1994