Weld bead and joint strength characteristics during laser welding of 87% AI2O3ceramics ‐ High‐power CO2laser welding of 87% Al2O3ceramics (1st report)
Authors:
- 1 January 1995
- journal article
- other
- Published by Taylor & Francis in Welding International
- Vol. 9 (8) , 615-620
Abstract
To develop a joining technology for thick ceramics, the fundamental characteristics of high‐power CO2 laser welding of 87% A12O3 ceramics have been investigated. The results suggest that a penetration depth of 20 mm is possible at a welding speed of 6.5 mm/sec and laser power of 10 kW. The porosity ratio is lower at lower input powers, also tending to decrease with a decreasing welding speed at the same input power. The bending strength decreases with an increasing porosity ratio. Porosities, especially large sink mark porosities at the bead centre, strongly affect the bending strength of welded joints in alumina ceramics. The root bending strength of 4 mm thick butt‐welded plate has the same value as the base material.Keywords
This publication has 2 references indexed in Scilit:
- Beam hole behaviour during laser beam welding1983
- Effect of Porosity on Physical Properties of Sintered AluminaJournal of the American Ceramic Society, 1956