Photopolymerization of product blending methyl methacrylate with reactive mesogen RM257 using the UV curing method

Authors:

Abstract
Photopolymerization of product blending methyl methacrylate with reactive mesogen RM257 using the UV Curing method with time variations. UV radiation formed a new polymer by adding the Benzoyl Peroxide (BPO) initiator. Polymerization was carried out at a temperature of 120°C in time variations of 5 minutes, 10 minutes, 15 minutes, and 20 minutes. Polymers were characterized using FTIR, SEM, XRD, and LCR Meter. FTIR spectrum showed the absorption peak at 2950 cm−1 indicating–C-H3 bonds, 1721 cm−1 indicating C=O bonds, 1604 cm−1 indicating aromatic functional group, 1248 cm−1 indicating C-O-C bonds, 1144 and 1060 cm−1 indicates of C-O bonds. Morphology analysis by SEM shows that polymer has uniform textures and visible molecular shape of rods. Pattern peaks of XRD appeared at an angle range of 2θ 10°-90°, there was a broad peak at 2θ 10°-38°, the appearance of sharp peaks with moderate intensity at 2θ 13.90° and 16.83°, high intensity appeared at 2θ 44.66°. This pattern XRD indicates that the polymer of product blending is semicrystalline. An LCR meter's measurement conductivities show that the highest conductivity value of a thin film is 2.245 x 10−6 S/cm.

This publication has 13 references indexed in Scilit: