Abstract
Background: Various types of crowns are used for full-coverage restoration of primary teeth affected by caries, developmental defects, or after pulp therapy. Prefabricated Stainless Steel and Zirconia crowns are commonly utilized. Bioflx crowns, which blend the properties of Stainless Steel and Zirconia, provide a flexible and aesthetically pleasing alternative. Aim: This study aimed to evaluate the vertical marginal gap and fracture resistance of Bioflx pediatric crowns compared to Zirconia and Stainless Steel crowns following thermomechanical aging. Methods: This in-vitro study was conducted using mandibular second primary crowns of three different materials (n = 30). Crowns were divided into three groups; Zirconia crowns group (n = 10, Nu Smile, USA), Bioflx crowns group (n = 10, Nu Smile, USA) and Stainless Steel crowns group (n = 10, Nu Smile, USA). The crowns were cemented onto standardized acrylic resin dies and subjected to thermomechanical aging. Vertical marginal gap measurements were obtained using a USB digital microscope with an integrated camera, while fracture resistance was assessed with a universal testing machine. Data were analyzed for outliers and tested for normality using the Shapiro-Wilk or Kolmogorov-Smirnov tests, with statistical significance set at 0.05. Results: Significant differences were observed in the vertical marginal gaps among the groups after cementation and thermomechanical aging (P = 0.013 and P = 0.001, respectively). Zirconia crowns exhibited the largest average marginal gap, followed by Bioflx and Stainless Steel crowns. Stainless steel crowns demonstrated the highest fracture resistance, followed by Bioflx crowns, while Zirconia crowns showed the lowest. Conclusions: Bioflx crowns exhibit the largest vertical marginal gap but show greater fracture resistance compared to Zirconia crowns, although they are still less resistant than Stainless Steel crowns after undergoing thermomechanical aging.Keywords
Funding Information
- Aswan University
This publication has 59 references indexed in Scilit:
- Zirconia crowns as an esthetic alternative for oral rehabilitation in pediatric dentistry: A reviewPediatric Dental Journal, 2021
- Effect of virtual cement gap settings on the marginal fit of cemented resin-ceramic crowns on implant abutmentsThe Journal of Prosthetic Dentistry, 2021
- Two-body wear and fracture behaviour of an experimental paediatric composite crown in comparison to zirconia and stainless steel crowns dependent on the cementation modeDental Materials, 2021
- Influence of ceramic firing on marginal gap accuracy and metal-ceramic bond strength of 3D-printed Co-Cr frameworksThe Journal of Prosthetic Dentistry, 2020
- In vitro comparison of microleakge between preformed metal crowns and aesthetic crowns of primary molars using different adhesive luting cementsEuropean Archives of Paediatric Dentistry, 2018
- Fracture resistance of CAD-CAM monolithic ceramic and veneered zirconia molar crowns after aging in a mastication simulatorThe Journal of Prosthetic Dentistry, 2018
- Guided tooth preparation for a pediatric zirconia crownThe Journal of the American Dental Association, 2018
- Marginal adaptation of zirconium dioxide copings: Influence of the CAD/CAM system and the finish line designThe Journal of Prosthetic Dentistry, 2014
- Thermal cycling for restorative materials: Does a standardized protocol exist in laboratory testing? A literature reviewJournal of the Mechanical Behavior of Biomedical Materials, 2014
- Fatigue strength of 316L-type stainless steel in simulated body fluidsCorrosion Science, 2011