Low‐modulus siloxane‐based polyurethanes. I. Effect of the chain extender 1,3‐bis(4‐hydroxybutyl)1,1,3,3‐tetramethyldisiloxane (BHTD) on properties and morphology
Authors:
- 20 November 2001
- journal article
- research article
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 83 (4) , 736-746
Abstract
A series of eight polyurethane elastomers was prepared using a two‐step bulk polymerization procedure to investigate the effect of the siloxane chain extender 1,3‐bis(4‐hydroxybutyl)1,1,3,3‐tetramethyldisiloxane (BHTD) on polyurethane properties and morphology. All polyurethanes were based on 40 wt % hard segment derived from 4,4′‐methylenediphenyl diisocyanate (MDI) and a mixture of 1,4‐butanediol (BDO) and BHTD in varying molar ratios. The soft segment was based on an 80 : 20 (w/w) mixture of the macrodiols α,ω‐bis(6‐hydroxyethoxypropyl)polydimethylsiloxane (PDMS, MW 965) and poly(hexamethylene oxide) (PHMO, MW 714). Polyurethanes were characterized by size‐exclusion chromatography, tensile testing, differential scanning calorimetry, dynamic mechanical thermal analysis, and FTIR spectroscopy. Clear and transparent polymers were produced in all cases with number‐average molecular weights in the range of 90,000 to 111,000. The ultimate tensile strength decreased only slightly (15%), but Young's modulus and flexural modulus decreased by 76 and 72%, respectively, compared with that of the pure BDO extended polyurethanes as the amount of BHTD was increased to 40 mol %. This change resulted in “softer” and more elastic polyurethanes. Polyurethanes with BHTD contents above 40 mol % were more elastic but had poor tensile and tear strengths. A 60 : 40 molar ratio of BDO : BHTD produced a “soft” polyurethane, which combined good tensile strength and flexibility. The DSC and DMTA results confirmed that the incorporation of BHTD as part of the hard segment yielded polyurethanes with improved compatibility between hard and soft segments. IR data indicated that the amount of hard segments soluble in the soft‐segment phase increased with increasing BHTD, contributing to the improved phase mixing. © 2002 Wiley Periodicals, Inc. J Appl Polym Sci 83: 736–746, 2002Keywords
This publication has 10 references indexed in Scilit:
- Poly(dimethylsiloxane)/poly(hexamethylene oxide) mixed macrodiol based polyurethane elastomers. I. Synthesis and propertiesJournal of Applied Polymer Science, 2000
- In-vivo degradation of polyurethanes: transmission-FTIR microscopic characterization of polyurethanes sectioned by cryomicrotomyBiomaterials, 1997
- Changes in structure and properties due to mechanical fatigue for polyurethanes containing poly(dimethyl siloxane)Polymer, 1994
- Synthesis and characterization of poly(siloxane‐urethane)sPolymer International, 1992
- Synthesis and characterization of hydroxy‐terminated poly(alkylene oxides) by condensation polymerization of diolsPolymer International, 1992
- Synthesis and characterization of polydimethylsiloxane polyurea‐urethanes and related zwitterionomersJournal of Polymer Science Part B: Polymer Physics, 1991
- Bulk, surface and blood-contacting properties of polyether polyurethanes modified with polydimetnylsiloxane macroglycolsBiomaterials, 1989
- Structure-property relationships and moisture sensitivity of PDMS/PTMO mixed soft segment urethane elastomersJournal of Macromolecular Science, Part B, 1988
- Poly(chloropropylmethyl‐dimethylsiloxane)–polyurethane elastomers: Synthesis and properties of segmented copolymers and related zwitterionomersJournal of Polymer Science Part B: Polymer Physics, 1986
- Ultimate Tensile Properties of Segmented Polyurethane Elastomers: Factors Leading to Reduced Properties for Polyurethanes Based on Nonpolar Soft SegmentsRubber Chemistry and Technology, 1986