Low-Temperature Stress Corrosion Cracking of Austenitic and Duplex Stainless Steels Under Chloride Deposits
Authors:
- Tomas ProsekTomas Prosek
- Anne Le GacAGAnne Le Gac
- Dominique ThierryDominique Thierry
- Sandra Le ManchetSMSandra Le Manchet
- Christian LojewskiCLChristian Lojewski
- Amelie FanicaAFAmelie Fanica
- Elisabeth JohanssonEJElisabeth Johansson
- Carolina CanderydCCCarolina Canderyd
- Francois DupoironFDFrancois Dupoiron
- Tom SnauwaertTSTom Snauwaert
- Fleur MaasFMFleur Maas
- Benny DroesbekeBDBenny Droesbeke
- 16 June 2014
- journal article
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 70 (10) , 1052-1063
Abstract
Corrosion performance of austenitic-ferritic (duplex) stainless steels UNS S32101, S32202, S32304, and S32205 and austenitic stainless steels UNS S30403 and S31603 was studied in the presence of chloride deposits simulating non-rinsing atmospheric conditions. The effect of temperature, relative humidity, concentration, and composition of the chloride deposits on the tendency for atmospheric, low-temperature, chloride-induced stress corrosion cracking (SCC), pitting, and selective corrosion was assessed using prestressed samples with a circular weld. In the presence of calcium chloride, SCC was observed at temperatures as low as 20°C and 30°C on the austenitic stainless steels UNS S30403 (Type 304L) and UNS S31603 (Type 316L), respectively. The only cases of SCC of tested duplex stainless steel grades were found at 70°C, which otherwise suffered mainly selective dissolution of the ferrite phase with one order lower depth of attack. The initiation of SCC and selective/pitting corrosion was governed by the equilibrium chloride concentration in a solution formed by contact with chloride-containing deposits and with air at a given relative humidity. Threshold levels of critical chloride concentrations, critical relative humidity in the presence of specific deposits, and maximum temperatures for safe applications of the studied grades were established.Keywords
This publication has 16 references indexed in Scilit:
- Failure analysis of a rock anchor made of stainless steel in marine environmentEngineering Failure Analysis, 2012
- Stress corrosion cracking of stainless-steel canister for concrete cask storage of spent fuelJournal of Nuclear Materials, 2008
- Marine Atmospheric SCC of Unsensitized Stainless Steel Rock Climbing ProtectionJournal of Failure Analysis and Prevention, 2008
- Stress Corrosion Cracking Growth Rates of Candidate Canister Materials for Spent Nuclear Fuel Storage in Chloride-Containing AtmosphereMATERIALS TRANSACTIONS, 2007
- Material selection of safety‐relevant components in indoor swimming poolsMaterials and Corrosion, 2003
- Untersuchungen zur Spannungsrißkorrosionsbeständigkeit nichtrostender Stähle mit unterschiedlichem VerformungsgradMaterials and Corrosion, 1999
- Chloridinduzierte Korrosion von nichtrostenden Stählen in Schwimmhallen-Atmosphären Teil 2: Einfluß von HypochloritenMaterials and Corrosion, 1998
- Chloridinduzierte Korrosion von Nichtrostenden Stählen in Schwimmhallen‐Atmosphären Teil 1: Elektrolyt Magnesium‐Chlorid (30%)Materials and Corrosion, 1997
- Room temperature stress corrosion cracking of stainless steels in indoor swimming pool atmospheresBritish Corrosion Journal, 1991
- Spannungsrißkorrosion nichtrostender austenitischer Chrom‐Nickel‐Stähle bei RaumtemperaturMaterials and Corrosion, 1989