Effect of pressure on the growth of boron and nitrogen doped HFCVD diamond films on WC–Co substrate
Authors:
- 23 January 2015
- journal article
- research article
- Published by Wiley in Surface and Interface Analysis
- Vol. 47 (5) , 572-586
Abstract
Boron and nitrogen compounds are added in the acetone/hydrogen gas mixture to deposit hot filament chemical vapor deposition (HFCVD) diamond films on the cobalt cemented tungsten carbide (WC–Co) substrate under the pressure of 1–4 kPa. The as‐deposited diamond films are characterized by field emission scanning electron microscope (FESEM), atomic force microscopy (AFM), X‐ray diffraction (XRD) spectroscopy and Raman spectroscopy. The results reveal that the surface morphology, growth rate, structure and quality of the diamond films vary with the pressure and the type of the impurity addition. The diamond grains tend to develop into the nanometer scale with the decrease of the pressure. However, adding of boron or nitrogen impurities in the gas mixture will weaken the nanocrystallization effect by reducing the carbon supersaturation. Density functional theory (DFT) calculations indicate that co‐adsorption of B and N containing radicals can favor the adsorption of CH 3 on diamond (100) surface. Thus, at low pressure of 1 kPa, large grained cubic (100) facet diamond rather than typical nanometer diamond is produced for B–N co‐addition gas mixture. The present results appear to be useful to efficiently synthesize high quality doped diamonds with desirable properties for mechanical application. Copyright © 2015 John Wiley & Sons, Ltd.Keywords
Funding Information
- National Natural Science Foundation of China (51275302, 51375011)
- Chenguang Program of Shanghai Municipal Education Commission (12CG11)
- Technical Innovation Funds for the Sci-Tech Enterprise of Jiangsu Province (BC2012124)
- Natural Science Foundation of Jiangsu Province (BK2012203)
This publication has 38 references indexed in Scilit:
- Influence of boron carbide on properties of CVD-diamond thin films at various deposition pressuresCurrent Applied Physics, 2012
- Diamond films with preferred texture by hot filament CVD at low pressureDiamond and Related Materials, 2008
- Tribological properties of undoped and boron-doped nanocrystalline diamond filmsThin Solid Films, 2008
- Boron doped diamond deposited by microwave plasma-assisted CVD at low and high pressuresDiamond and Related Materials, 2008
- Growth rate improvements in the hot-filament CVD deposition of nanocrystalline diamondDiamond and Related Materials, 2006
- SEM and Raman analysis of boron-doped diamond coating on spherical textured substratesSurface and Coatings Technology, 2006
- Characterization of boron doped CVD diamond films by Raman spectroscopy and X-ray diffractometryDiamond and Related Materials, 2002
- Dependence of the growth rate, quality, and morphology of diamond coatings on the pressure during the CVD-process in an industrial hot-filament plantDiamond and Related Materials, 2002
- A study of the crystalline growth of highly boron-doped CVD diamond: preparation of graded-morphology diamond thin filmsDiamond and Related Materials, 2001
- Stress study of HFCVD boron-doped diamond films by X-ray diffraction measurementsDiamond and Related Materials, 2001