Effect of low-temperature preannealing on laser-annealed p+/n ultrashallow junctions
Authors:
- 1 April 2002
- journal article
- conference paper
- Published by AIP Publishing in Applied Physics Letters
- Vol. 80 (13) , 2272-2274
Abstract
The effect of low-temperature preannealing on ultrashallow junctions was examined. An ultrashallow junction was formed by means of plasma doping at an energy of 500 V. The junction was activated by low-temperature (300–500 °C) annealing, followed by laser annealing. Compared with control samples which were not preannealed, low-temperature preannealing significantly improves junction characteristics, resulting in a reduction in junction depth and a lower leakage current density. A cross-sectional transmission-electron-microscopy analysis confirmed the lower defect density, which explains the lower leakage current. By optimizing the process conditions, excellent electrical characteristics of the junction, i.e., a junction depth of 28 nm and a sheet resistance of 250 Ω/sq, can be obtained.
Keywords
This publication has 4 references indexed in Scilit:
- Annealing of ultrashallow p+/n junction by 248 nm excimer laser and rapid thermal processing with different preamorphization depthsApplied Physics Letters, 2000
- Characterization of sub-30 nm p[sup +]/n Junction Formed by Plasma Ion ImplantationJournal of the Electrochemical Society, 2000
- Boron-enhanced diffusion of boron from ultralow-energy ion implantationApplied Physics Letters, 1999
- Improved Characteristics of p+-n Junctions formed by Excimer Laser Annealing with Low Temperature Pre-AnnealingJapanese Journal of Applied Physics, 1996