Evolution of Spheroidized Annealing Microstructure and Toughening Mechanism of High Si-Al Pearlitic Bearing Steel

Authors:

Abstract
This study systematically investigates the mechanism underlying the effects of combined addition of Si and Al on the microstructure evolution during spheroidizing annealing and the strength-toughness properties of GCr15 bearing steel. The results indicate that Si–Al alloying increases the austenitization temperature (Ac1) and austenite stability, thereby significantly refining the initial pearlitic microstructure and reducing the pearlite interlamellar spacing from 655 nm to 431 nm. However, as non-carbide-forming elements, Si and Al also decrease carbon diffusivity and retard spheroidization kinetics. This leads to incomplete spheroidization under the same annealing conditions, resulting in a mixed carbide morphology consisting of spherical carbides and residual lamellar carbides. Regarding the strengthening and toughening mechanism, the addition of Si–Al significantly improves the strength through grain refinement strengthening and pearlite refinement. After spheroidizing annealing, the Si–Al bearing steel retains a considerable degree of solid-solution strengthening, resulting in a strength reduction of only 2.6%, which is superior to the 11.0% decrease in the steel without Si–Al addition. The improvement in impact toughness is mainly attributed to the increased proportion of high-angle grain boundaries and the optimized carbide morphology, which transforms from a continuous network into dispersed particles, thereby effectively restraining crack propagation. Si–Al alloying refines the microstructure while retarding the spheroidization process, providing an important theoretical basis for developing high-efficiency and energy-saving heat treatment processes for bearing steels.

This publication has 16 references indexed in Scilit: