Laser Metal Deposition of Aluminum Alloys 7075 and 5083 with the Addition of Volatile Alloying Elements through Powder Blending
Open Access
- 31 January 2026
- journal article
- Published by Wiley in Advanced Engineering Materials
- Vol. 28 (7)
Abstract
Laser metal deposition (LMD) offers high flexibility in material selection. However, processing high‐strength aluminum alloys, like EN AW‐7075, remains challenging due to limited weldability and the evaporation of volatile alloying elements. In this work, solidification cracking is mitigated through grain refinement using TiC nanoparticle as nuclei. The evaporation of zinc and magnesium compromises precipitation‐hardening and solid‐solution‐hardening capacity and thus mechanical properties. This issue is addressed by in situ and ex situ powder blending with additional high Zn and Mg powders, such as ZnAl12 and AZ91. LMD of EN AW‐7075 results in losses of up to 65% Zn and 60% Mg, while EN AW‐5083 shows Mg losses of up to 35%. It is found that the majority of the additional Zn and Mg powders is lost through evaporation, necessitating increased additions. With an addition of 10% ZnAl12 and 5% AZ91, the EN AW‐7075 samples reach a composition according to the standard and are suitable for a heat treatment following T6. With an addition of 10% AZ91, the EN AW‐5083 samples reach a composition desired composition. This strategy highlights the potential for extending the range of processable aluminum alloys in additive manufacturing and opens pathways for the application of high‐strength alloys, such as EN AW‐7075.Keywords
Funding Information
- Deutsche Forschungsgemeinschaft (434424600)
This publication has 20 references indexed in Scilit:
- Laser metal deposition (LMD) of 7075 aluminum alloy with minimized defects: Process, microstructure and mechanical propertiesJournal of Alloys and Compounds, 2025
- Hybrid heat-source solid-state additive manufacturing: A method to fabricate high performance AA6061 depositionJournal of Materials Science & Technology, 2025
- Laser metal deposition of Al 7075: Effects of TiC nanoparticlesJournal of Materials Research and Technology, 2024
- High‐throughput preparation for alloy composition design in additive manufacturing: A comprehensive reviewMaterials Genome Engineering Advances, 2024
- High‐Throughput Alloy Development Using Advanced Characterization Techniques During Directed Energy Deposition Additive ManufacturingAdvanced Engineering Materials, 2023
- The microstructures and mechanical properties of Al-Zn-Mg-Cu-Si-Zr alloy: A comparison between directed energy deposition and laser powder bed fusionMaterials Letters, 2023
- Laser based additive manufacturing in industry and academiaCIRP Annals, 2017
- Changing the alloy composition of Al7075 for better processability by selective laser meltingJournal of Materials Processing Technology, 2016
- Roles of Alloy Composition and Grain Refinement on Hot Tearing Susceptibility of 7××× Aluminum AlloysMetallurgical and Materials Transactions A, 2016
- Interfacial phenomena in wettability of TiC by Al–Mg alloysActa Materialia, 2004