Low temperature sintering and elongated grain growth of 6H-SiC powder with AlB2 and C additives

Authors:
  • HTHidehiko Tanaka
    Hidehiko Tanaka
  • YZYou Zhou
    You Zhou

Abstract
6H(α)-SiC fine powder was sintered at normal pressure with additives of between 0.67 to 2.7 wt.% of AlB2 and 2 wt.% of C. The powder could be densified at 1850 °C. This sintering temperature was lower than that for SiC with B and C additives by 150–300 °C. During sintering, 6H-SiC partially transformed into 4H-SiC, and the transformation caused grain to grow and develop a nonspherical shape. The fracture toughness of sintered SiC increased with increases in the amount of AlB2 additive, the mean grain size, and the mean aspect ratio of grain shape. AlB2 and C additives are believed to have formed an Al8B4C7 compound which melted below 1800 °C and enhanced sintering and grain growth.
Keywords

This publication has 52 references indexed in Scilit: