Oxygen isotopic exchange between an 18O+ implanted Si layer and a natural SiO2 capping layer during high-temperature annealing

Authors:

Abstract
To understand the effects of the SiO2 capping layer on the growing buried SiO2 layer a silicon wafer was implanted at 680 °C with 90 keV 18O+ to a dose of 4.3×1017 18O+/cm2. After the deposition of an ∼500 nm natural SiO2 cap by the plasma sputtering, one piece of the implanted wafer was annealed at 1360 °C for 6 h in a quartz silica tube in flowing nitrogen. There is clear evidence of diffusional mixing of the oxygen isotopes from the cap into the 18O+ implanted layer during this annealing step, indeed a surprisingly large amount has taken place, in that approximately 41% of 18O contained within the buried SiO2 layer has been exchanged with the cap.