Processing of sodium-potassium niobate ceramics

Authors:
  • JRJr
    Jr
  • BRBob R.
    Bob R.

Abstract
Sintering studies of undoped (Na 0.5K 0.5)NbO 3 and the same material doped with 1/2, 1, 2, and 4 mole percent BaO and 2 mole % B 2O 3 were made. The persistence of a second phase after calcining to form the compound led to a study of reactions occurring during calcination. The calcining of sodium-potassium niobates involves the formation of an intermediate compound (the second phase) and its subsequent reaction with sodium oxide and potassium oxide to form (Na 0.5K 0.5)NbO 3. Sintering data show that up to 1/2 mole % BaO added to the system increases the initial densification. However, the sintered bodies then exhibit densification and form sharp cubic grains and large voids. Indications are that a liquid phase is the major contributor to densification of this system through the mechanism of particle rearrangement, and that the contribution of any sintering mechanism to densification is negligible.
Funding Information
  • US Atomic Energy Commission (AEC)
  • DOE (W-7405-ENG-48)