HVEM Observations of Crack Tip Produced in Type 304 Stainless Steel by SCC and HE

Authors:
  • TNTakenori Nakayama
    Takenori Nakayama

Abstract
Using a high voltage electron microscope (HVEM), observations of stress corrosion crack tips of a sheet specimen of Type 304 stainless steel in 2.5 mol/l H2SO4 + 0.5 mol/l NaCl at room temperature and of a rod specimen In 20% NaCl at 100 C have been carried out and hydrogen embrittlement crack tips of a hydrogen precharged sheet specimen has also been observed, to clarify the propagation mechanism of stress corrosion cracking (SCC) in these corrosive environments and hydrogen embrittlement (HE). Furthermore, the effects of crosshead speed and prestrain on the SCC behavior were examined by a slow strain rate technique (SSRT). Their fracture surfaces were also observed by a scanning electron microscope. For SCC in 2.5 mol/l H2SO4 + 0.5 mol/l NaCl, the stress corrosion fracture surfaces of the sheet and rod specimens both changed from a fine parallel pleat pattern to a parallel groove attack, with increasing stress level. It has been found that in case of low stress levels, the crack propagation would be performed mainly by a preferential dissolution of active slip planes containing numerous moving dislocations under straining, and the fine parallel pleat pattern on the fracture surface could be attributed to this propagation process. In case of high stress levels or prestrained specimens, the possibilities of a preferential dissolution or an HE of martensite phases (α', ϵ) induced by applied stress and/or hydrogen generated by corrosion have also been shown for the crack propagation. In this case, the parallel groove attack on the fracture surface could be attributed to a dissolution of martensite phases. For SCC in 20% NaCl, the fracture surface was mainly characterized by a fine parallel pleat pattern. It has been found that the crack could be produced by the preferential attack of the active slip planes, while α'-martensite was occasionally observed near a crack. On the other hand, the fracture surface of HE was similar to that of SCC, in that fine pleats and steps were recognized. HVEM observations of the crack tips, however, revealed that the HE crack propagated mainly along ϵ-martensite and partly in the region having a mixed structure of α' and ϵ-phases.

This publication has 25 references indexed in Scilit: