Oxidation of SiOC Composite Having Dispersoids of Mo4.8Si3C0.6 and MoSi2
Authors:
- 15 June 2005
- journal article
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 486-487, 165-168
Abstract
New ceramic composites that consist of the amorphous SiOC matrix having dispersoids of Mo4.8Si3C0.6 and some MoSi2 were synthesized, and their oxidation characteristics were investigated between 450 and 1050oC in air. The SiOC matrix was obtained by converting polymethylsiloxane via pyrolysis. The good oxidation resistance of the prepared composites originated from a thin, protective SiO2 layer formed on the surface. But the outermost oxide surface was porous, owing to the formation of the highly volatile MoO3, which was formed together with SiO2.Keywords
This publication has 7 references indexed in Scilit:
- Simultaneous equivariant estimation of the parameters of matrix scale and matrix location-scale modelsStatistical Papers, 2005
- Oxidation of SiOC/MoSi2/SiC Composites Prepared by Polymer PyrolysisOxidation of Metals, 2004
- High temperature oxidation and pesting of Mo(Si,Al)2Materials Science and Engineering: A, 1997
- Active‐Filler‐Controlled Pyrolysis of Preceramic PolymersJournal of the American Ceramic Society, 1995
- Microstructure Development of Oxycarbide Composites during Active‐Filler‐Controlled Polymer PyrolysisJournal of the American Ceramic Society, 1993
- High‐Temperature Oxidation of Molybdenum DisilicideJournal of the American Ceramic Society, 1966
- High-Temperature OxidationJournal of the Electrochemical Society, 1965