Microstructure Evolution and Deformation Mechanisms of As-Cast Antibacterial Ti6Al4V-5Cu Alloy for Isothermal Forging Process
Open Access
Abstract
The hot workability behavior of antibacterial Ti6Al4V-5Cu alloy was investigated using a hot compression experiment in the temperature range of 790–1040 °C and strain rate of 10−3–10 s−1 with a strain of 0.4. The deformation behavior of the alloy was characterized by Gleeble 3800 compression experiment, and the relationship among deformed microstructures and deformation parameters was established. The deformations of Ti6Al4V-5Cu alloy were temperature and strain rate-dependent. Higher temperature and lower strain rate made power dissipation efficiency (η) increase and reach 89%. The activation energies (Q) in the dual-phase (α + β) and single β phase regions were calculated as 175.43 and 159.03 kJ mol−1, respectively. In the dual (α + β) phase region, with an increase in strain rate, flow-softening behavior was dominated, however in the single β phase region such as processing at 940 °C. Flow stress increased slightly in which work-hardening behavior was dominated (especially between strain rates of 10−3–1 s−1). The deformation at various conditions exhibited different stress-strain profiles, providing an insight that work hardening and flow softening coexisted in Ti6Al4V-5Cu alloy. The relative intensity of oscillatory change in flow stress profile decreased as the strain rate decreased. The hot workability of Ti6Al4V-5Cu alloy was also accessed from the viewpoint of the sub-grain structure.Keywords
Funding Information
- Research and Development Program of the CAS-WEGO Group
This publication has 39 references indexed in Scilit:
- Flow stress behavior of commercial pure titanium sheet during warm tensile deformationMaterials & Design (1980-2015), 2012
- Introduction of antibacterial function into biomedical TiNi shape memory alloy by the addition of element AgActa Biomaterialia, 2011
- Effect of hot working on flow behavior of Ti–6Al–4V alloy in single phase and two phase regionsMaterials & Design (1980-2015), 2010
- Workability of Ti–6Al–4V alloy at high temperatures and strain ratesMaterials Letters, 2004
- Deformation behavior of beta-titanium alloysMaterials Science and Engineering: A, 2003
- Characterization of deformation stability in hot forging of conventional Ti–6Al–4V using processing mapsJournal of Materials Processing Technology, 2002
- Mechanical behavior of Ti–6Al–4V at high and moderate temperatures—Part I: Experimental resultsMaterials Science and Engineering: A, 2002
- Hot working of commercial Ti–6Al–4V with an equiaxed α–β microstructure: materials modeling considerationsMaterials Science and Engineering: A, 2000
- Hot deformation and microstructural damage mechanisms in extra-low interstitial (ELI) grade Ti–6Al–4VMaterials Science and Engineering: A, 2000
- The use of titanium for medical applications in the USAMaterials Science and Engineering: A, 1996