Abstract
Most commercial Ni-based alkaline batteries use β-Ni(OH)2 as the cathode material. These batteries are particularly attractive due to the use of low-cost materials and nonflammable aqueous electrolytes, which enhance safety and recyclability. However, these electrodes suffer from structural instability during charge–discharge cycles caused by phase transitions between β-Ni(OH)2/β-NiOOH and α-Ni(OH)2/γ-NiOOH redox couples, leading to capacity fading over time. Therefore, stabilizing the β polymorph remains a significant challenge. In this study, nickel hydroxyfluorides (Ni(OH)2–xFx) were synthesized using microwave-assisted hydrothermal routes. It was possible to increase the fluorine content up to 0.48 while maintaining the β-Ni(OH)2 structural type. Powder X-ray diffraction and vibrational spectroscopy (FTIR, Raman) revealed substantial structural variations with fluorine incorporation. The highly electronegative fluorine plays a crucial role in enhancing both intraslab interactions, by increasing lattice rigidity, and interslab interactions, by affecting the level of the O–H bonds and H–H electrostatic repulsion. UV–vis–NIR spectroscopy confirmed the increased bond ionicity of the fluorinated samples, evidenced by an optical bandgap opening, a decrease of crystal field stabilization energy, and a slight increase of the Racah parameter. Thermogravimetric analysis showed a gradual increase in the decomposition temperature with higher fluorine content. Interestingly, the thermal decomposition of nickel hydroxyfluorides resulted in a novel synthesis method for nickel oxyfluorides (Ni1–(y/2) □y/2O1–yFy), stabilizing nickel vacancies. Galvanostatic cycling tests indicated a significant capacity decrease in the fluorine-containing samples. To further understand the mechanisms behind the reduced electrochemical performance, chemical oxidation tests were conducted. These tests demonstrated the inability of the fluorinated samples to be oxidized, suggesting that the high electronegativity of fluorine prevents nickel oxidation.Keywords
Funding Information
- Agence Nationale de la Recherche
This publication has 51 references indexed in Scilit:
- Stacking fault disorder induced by Mn doping in Ni(OH)2 for supercapacitor electrodesChemical Engineering Journal, 2021
- Cabbage-like α-Ni(OH)2 with a good long-term cycling stability and high electrochemical performances for supercapacitor applicationsChemical Physics Letters, 2017
- Absorption spectroscopy of octahedral nickel(II) complexes: A case study of interactions between multiple electronic excited statesCoordination Chemistry Reviews, 2007
- Physical characterization, electrochemical performance and storage stability of spherical Al-substituted γ-NiOOHElectrochimica Acta, 2007
- Raman spectroscopic study of hydroxyl-clinohumite at various pressures and temperaturesPhysics and Chemistry of Minerals, 2000
- New manganese-substituted nickel hydroxidesJournal of Power Sources, 1994
- Lattice vibration spectra. Part LXXXII. Brucite-type hydroxides M(OH)2 (M = Ca, Mn, Co, Fe, Cd) — IR and Raman spectra, neutron diffraction of Fe(OH)2Journal of Molecular Structure, 1994
- Weak hydrogen bonds in solid hydroxides and hydratesJournal of Molecular Structure, 1994
- Spectroscopic study of nickel hydroxyde, nickel carbonate-hexahydrate and nickel hydroxocarbonateJournal of Molecular Structure, 1984
- Zur kenntnis der nickelhydroxidelektrode—I.Über das nickel (II)-hydroxidhydratElectrochimica Acta, 1966