Debye temperature of 4 H -SiC determined by X-ray powder diffraction
- 1 December 2009
- journal article
- research article
- Published by Cambridge University Press (CUP) in Powder Diffraction
- Vol. 24 (4) , 311-314
Abstract
Crystal structure of 4 H -SiC was refined from room-temperature X-ray powder diffraction data using the Rietveld refinement method. The refined lattice constants were determined to be a = b =3.079 93(0) Å, c =10.082 22(2) Å, and the refined overall temperature factor B =0.383(3) Å 2 . Using the Debye approximation, the Debye temperature was successfully determined to be 1194.8 K.Keywords
This publication has 16 references indexed in Scilit:
- Factors affecting the formation of misoriented domains in 6H‐SiC single crystals grown by PVT methodCrystal Research and Technology, 2009
- Silicon Carbide Crystal and Substrate Technology: A Survey of Recent AdvancesMaterials Science Forum, 2004
- An analysis of seed graphitization for sublimation growth of SiC bulk crystalDiamond and Related Materials, 2004
- Factors affecting the graphitization behavior of the powder source during seeded sublimation growth of SiC bulk crystalJournal of Crystal Growth, 2003
- Influence of polytypism on thermal properties of silicon carbidePhysical Review B, 1996
- X-ray Rietveld Analysis with a Physically Based BackgroundJournal of Applied Crystallography, 1995
- Debye temperatures for hexagonal crystalsPhysical Review B, 1981
- A profile refinement method for nuclear and magnetic structuresJournal of Applied Crystallography, 1969
- A review of the structure of silicon carbideActa Crystallographica Section B: Structural Science, Crystal Engineering and Materials, 1969
- Line profiles of neutron powder-diffraction peaks for structure refinementActa Crystallographica, 1967