Abstract
The crystalline powders of the LiNbO3 were studied. Measurements were carried out on the reference modified by the leaching procedure samples. Leaching reactions were conducted in the redistilled water and in the concentrated nitric acid. The Li+/H+ substitution was confirmed, for the crystal sample leached in nitric acid, by using time of flight-secondary ion mass spectroscopy (SIMS). The concentration of the lithium and niobium in liquid solutions was determined by using an inductively coupled plasma-optical emission spectrometry (ICP-OES). The X-ray diffraction (XRD) test was performed to verify the stability of the crystallographic structure of the powders, affected by the leaching procedure. For sample leached in the concentrated nitric acid, XRD pattern showed a structural distortion. The influence of the leaching reaction on the electric permittivity, conductivity and the coefficient loss was checked. The spectra were obtained for the frequency range 20–106 Hz, in the temperature range 300–650 K.