Influence of Bio-C and AH Plus sealers on bond strength determined by push-out of a fiberglass post installed with self-adhesive sealer
Authors:
- Lilian Tg AguiarLALilian Tg Aguiar
- Silvia Mbs SakamotoSSSilvia Mbs Sakamoto
- Carlos E FontanaCFCarlos E Fontana
- Rina A PelegrineRPRina A Pelegrine
- Renata O AmaralRARenata O Amaral
- Ana G LimoeiroALAna G Limoeiro
- Wayne M NascimentoWNWayne M Nascimento
- Daniel Gp RochaDRDaniel Gp Rocha
- Marília Fv Marceliano-AlvesMMMarília Fv Marceliano-Alves
- Alexandre S MartinAMAlexandre S Martin
- Carlos Es BuenoCBCarlos Es Bueno
Open Access
- 30 August 2025
- journal article
- Published by Sociedad Argentina de Investigacion Odontologica in Acta Odontológica Latinoamericana
- Vol. 38 (2) , 129-137
Abstract
Given the limitations of the intrarradicular adhesion procedure and the significant challenge of achieving effective bonding, it is essential to assess the potential impact of various endodontic sealers on the bond strength between fiberglass posts and root dentin. Aim: The aim of this study was to evaluate the bond strength of fiberglass posts to the root dentin of teeth filled with different endodontic sealers. Material and Methods: Forty-five single-rooted teeth were instrumented, filled using the single-cone technique, and divided into three groups according to the selected sealer (n=15): Bio-C sealer (GBC), AH Plus (GAH), and control group without sealer (GC). The post was installed using RelyX U200 self-adhesive resin sealer. Specimens were cut into a cervical, middle and apical thirds, to analyze one slice per third. Bond strength was evaluated using a push-out extrusion test. The failure modes in each third were observed under the microscope, and classified as adhesive, cohesive or mixed. Results: It was found a difference between groups in the cervical and apical thirds, with GAH having stronger adhesion in the cervical third than GBC (p=0.0015), although there was no difference with GC. In the apical third, GAH had higher adhesion values than GBC (p=0.0014) and GC (p=0.0005). In the middle third, there was no difference between groups (p=0.1386). The same sealer in the different thirds only differed significantly in the GBC group, where bond strength was higher in the middle and apical thirds, with a significant difference from the cervical third (p0.05). Conclusion: The predominant failure between dentin and sealer was adhesive. It was concluded that the use of AH Plus endodontic sealer resulted in less impairment of the bond strength of resin cemented fiberglass posts compared to bioceramic sealer.Keywords
This publication has 23 references indexed in Scilit:
- Influence of Using Clinical Microscope as Auxiliary to Perform Mechanical Cleaning of Post Space: A Bond Strength AnalysisJournal of Endodontics, 2015
- Comparison of Different Dentin Pretreatment Protocols on the Bond Strength of Glass Fiber Post Using Self-etching AdhesiveJournal of Endodontics, 2015
- Effect of the Type of Endodontic Sealer on the Bond Strength Between Fiber Post and Root Wall Dentin2014
- The Role of Resin Cement on Bond Strength of Glass-fiber Posts Luted Into Root Canals: A Systematic Review and Meta-analysis of In Vitro StudiesOperative Dentistry, 2014
- Influence of Endodontic Sealer Composition and Time of Fiber Post Cementation on Sealer Adhesiveness to Bovine Root DentinBrazilian Dental Journal, 2013
- Retention of fiber posts in different dentin regions: An in vitro studyIndian Journal of Dental Research, 2012
- The effect of calcium silicate‐based sealer on the push‐out bond strength of fibre postsAustralian Dental Journal, 2012
- The adhesive system and root canal region do not influence the degree of conversion of dual resin cementJournal of Applied Oral Science, 2010
- Influence of endodontic sealer cement on fibreglass post bond strength to root dentineInternational Endodontic Journal, 2008
- A comparison of canal preparations in straight and curved root canalsOral Surgery, Oral Medicine, Oral Pathology, 1971