Microstructure and Mechanical Characteristics of Ti-Ta Alloys before and after NaOH Treatment and Their Behavior in Simulated Body Fluid
Open Access
Abstract
In the present study, the microstructure and mechanical properties of Ti-xTa (x = 5%, 15%, and 25% wt. Ta) alloys produced by using an induced furnace by the cold crucible levitation fusion technique were investigated and compared. The microstructure was examined by scanning electron microscopy and X-ray diffraction. The alloys present a microstructure characterized by the α′ lamellar structure in a matrix of the transformed β phase. From the bulk materials, the samples for the tensile tests were prepared and based on the results and the elastic modulus was calculated by deducting the lowest values for the Ti-25Ta alloy. Moreover, a surface alkali treatment functionalization was performed using 10 M NaOH. The microstructure of the new developed films on the surface of the Ti-xTa alloys was investigated by scanning electron microscopy and the chemical analysis revealed the formation of sodium titanate and sodium tantanate along with titanium and tantalum oxides. Using low loads, the Vickers hardness test revealed increased hardness values for the alkali-treated samples. After exposure to simulated body fluid, phosphorus and calcium were identified on the surface of the new developed film, indicating the development of apatite. The corrosion resistance was evaluated by open cell potential measurements in simulated body fluid before and after NaOH treatment. The tests were performed at 22 °C as well as at 40 °C, simulating fever. The results show that the Ta content has a detrimental effect on the investigated alloys’ microstructure, hardness, elastic modulus, and corrosion behavior.Keywords
Funding Information
- Cabildo de Gran Canaria (CABINFR2019-07, SI-1821)
- Spanish Ministry of Universities (CABINFR2019-07, SI-1821)
- European Union, Maria Zambrano (CABINFR2019-07, SI-1821)
This publication has 32 references indexed in Scilit:
- Comparison of titanium soaked in 5M NaOH or 5M KOH solutionsMaterials Science and Engineering: C, 2013
- Preparation of bioactive Ti metal surface enriched with calcium ions by chemical treatmentActa Biomaterialia, 2010
- Elastic modulus measurement—obtaining reliable data from the tensile testMetrologia, 2010
- Comparative corrosion study of Ti–Ta alloys for dental applicationsActa Biomaterialia, 2009
- Ti–25Ta alloy with the best mechanical compatibility in Ti–Ta alloys for biomedical applicationsMaterials Science and Engineering: C, 2009
- Characterization of Ti‐Ta Alloys Synthesized by Cold Crucible Levitation MeltingAdvanced Engineering Materials, 2008
- A protocol to develop crack-free biomimetic coatings on Ti6Al4V substratesJournal of Materials Research, 2007
- Effects of Ta content on Young’s modulus and tensile properties of binary Ti–Ta alloys for biomedical applicationsMaterials Science and Engineering: A, 2004
- Preparation and characterization of Ti–Ta alloys for application in corrosive mediaMaterials Letters, 2003
- Mechanism of Apatite Formation on Bioactive Tantalum Metal in Simulated Body FluidKey Engineering Materials, 2003