Investigation of the surface residual stresses in spray cooled induction hardened gearwheels
- 1 January 2012
- journal article
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 103 (1) , 73-79
Abstract
The objective of the current investigation consists of testing the interchangeability of polymer solutions used during induction hardening with water – air spraying regarding compressive residual stresses. Gearwheels made of 42CrMo4 steel were induction hardened and subsequently quenched using water–air spray cooling. The effect of different cooling parameters on the surface's residual stresses in the gearwheel's tooth flanks was analysed by means of X-ray diffraction. The microstructure was characterised by means of hardness measurements and light-microscopy. Residual stresses could be specified after using water – air spray cooling and are comparable to those using polymer quenching. Quench parameters leading to maximum compressive residual stresses in tooth flanks were determined.Keywords
This publication has 7 references indexed in Scilit:
- Induction Hardening of Spur Gearwheels Made from 42CrMo4 Hardening and Tempering Steel by Employing Spray CoolingSteel Research International, 2010
- Eigenspannungen als Messgröße zur QualitätssicherungMaterialwissenschaft und Werkstofftechnik, 2007
- Overview of residual stress after quenching. Part II: factors affecting quench residual stressesInternational Journal of Materials and Product Technology, 2005
- Eigenspannungen und VerzugHTM Journal of Heat Treatment and Materials, 1996
- Induktives Randschichthärten von Stahl Ck 45 durch Abschrecken in zerstäubtem WasserHTM Journal of Heat Treatment and Materials, 1989
- Kriterien für die Auswahl des Abschreckmittels für das induktive RandschichthärtenHTM Journal of Heat Treatment and Materials, 1989
- Entstehung von Eigenspannungen und Verzügen bei der induktiven Randschichthärtung von BauteilenHTM Journal of Heat Treatment and Materials, 1989