Corrosion Characteristics of 2205 Duplex Stainless Steel in High Temperature and High Pressure Environment Containing H2S/CO2
Authors:
- 1 November 2012
- journal article
- Published by Trans Tech Publications, Ltd. in Applied Mechanics and Materials
- Vol. 236-237, 95-98
Abstract
The corrosion characteristics of 2205 duplex stainless steel in high- temperature and high-pressure (HT and HP) environments containing H2S/CO2 are investigated in this paper. After corroded 720 hours in the condition of 3.5 MPa H2S, 3.5 MPa CO2, 205°C, 15% NaCl and a sulfide content of 3g/L, one layer of comparably thick corrosion product are formed on the surface of the specimens. The corrosion products, which are relatively porous, lose its protection to the matrix. Lots of pitting are found on the surface of the steel and intercrystalline fracture and transcrystalline fracture are generated in the bottom of the pitting, which indicates its high sensitivity to stress corrosion crack (SSC). Also, the phenomenon of selective corrosion, a priority corrosion of α phase and minor corrosion or non-corrosion of γ phase, is observed after the corrosion process.Keywords
This publication has 8 references indexed in Scilit:
- Evaluation of environment-assisted cracking susceptibility of a grade X100 pipeline steelCorrosion Science, 2012
- Hydrogen trapping in an API 5L X60 steelCorrosion Science, 2012
- Corrosion Electrochemical Characteristics of the Passive Films Formed on Inconel 718 Alloy in the Environments Containing High H2S and CO2 Partial PressuresNanoscience and Nanotechnology Letters, 2011
- The non-linear fitting method to analyze the measured M–S plots of bipolar passive filmsElectrochimica Acta, 2010
- Effects of hydrogen on the fracture toughness of a X70 pipeline steelCorrosion Science, 2009
- 22 Cr 5 Ni duplex and 25 Cr 7 Ni superduplex stainless steel: Hydrogen influence on fatigue crack propagation resistanceEngineering Fracture Mechanics, 2008
- Investigation of hydrogen induced cracking in 2205 duplex stainless steel in wet H2S environments after isothermal treatment at 675, 750 and 900°CMaterials Characterization, 2006
- Quantitative fractography of 2205 duplex stainless steel after a sulfide stress cracking testMaterials Characterization, 2006