Properties of High-Strength Flowable Mortar Reinforced with Palm Fibers
Open Access
- 18 January 2012
- journal article
- Published by Hindawi Limited in ISRN Civil Engineering
- Vol. 2012, 1-5
Abstract
This study was conducted to determine some physical and mechanical properties of high-strength flowable mortar reinforced with different percentages of palm fiber (0, 0.2, 0.4, 0.6, 0.8, 1.0, 1.2, 1.4, and 1.6% as volumetric fractions). The density, compressive strength, flexural strength, and toughness index were tested to determine the mechanical properties of this mortar. Test results illustrate that the inclusion of this fiber reduces the density of mortar. The use of 0.6% of palm fiber increases the compressive strength and flexural strength by about 15.1%, and 16%, respectively; besides, the toughness index (I5) of the high-strength flowable mortar has been significantly enhanced by the use of 1% and more of palm fiber.Keywords
This publication has 5 references indexed in Scilit:
- High strength characteristics of cement mortar reinforced with hybrid fibresConstruction and Building Materials, 2011
- Development of high strength flowable mortar with hybrid fiberConstruction and Building Materials, 2010
- Impact strength of a few natural fibre reinforced cement mortar slabs: a comparative studyCement and Concrete Composites, 2005
- Development of vegetable fibre–mortar composites of improved durabilityCement and Concrete Composites, 2003
- Sugar cane bagasse fibre reinforced cement composites. Part I. Influence of the botanical components of bagasse on the setting of bagasse/cement compositeCement and Concrete Composites, 2003