The susceptibility of stress corrosion cracking (SCC) of Ni base alloys and 316 stainless steel was studied in less-oxidizing or reducing supercritical water (SCW) environments for determining the suitability of these alloys in the upgrading of low-quality hydrocarbon resources process. The cracking susceptibility of 316 stainless steel, UNS N06625(Alloy 625), UNS N10276(Alloy C-276) and MC-alloy (Ni-45Cr-1Mo) was investigated using slow strain rate test (SSRT) in supercritical water containing hydrogen chloride. All tests were performed at 400°C/25MPa. SCC did not occur in the deionized water at 400C°/25MPa. In less-oxidizing SCW with 0.001mol/l HCl, cracking occurred in type 316 stainless steel. With 0.001mol/lHCl, cracking occurred in Alloy C-276. With 0.01mol/l HCl, cracking occurred on Alloy 625. But SCC of MC alloy did not occur at these conditions. Cracking susceptibility of Ni base alloys decreased with increasing Cr content of alloys in less-oxidizing SCW containing HCl. In reducing atmosphere, the susceptibilities of SCC of these alloys were decreased with increasing hydrogen gas partial pressure.