Stress in Vacuum-Deposited Films of Ag, Au, and Cu

Authors:

Abstract
The tension per unit width of the film S has been determined for Ag, Au, and Cu films deposited at 10−5 Torr from a few tens of angstroms up to 2000, 1500, and 1000 Å in thickness, respectively. S increases rapidly with the film thickness d until the film attains a thickness dI( = 220/320/160 Å for Ag/Au/Cu films deposited at 2 Å/sec). At dI the mean stress within the film σ ( = S/d) assumes a maximum. With thicker Ag and Cu films S remains nearly constant until at a thickness dII it starts to increase again. With Au films the rapid increase in S below dI is immediately followed by a slower increase with d. The first increase in S below dI is associated with the coalescence of islands. The second increase in S observed at larger thicknesses (d > dII for Ag and Cu, d > dI for Au) is probably due to residual gases. The last view is supported by experiments with Ag films deposited at 10−8 Torr.