Preparation of Lead-Free Piezoelectric Ceramics from (1−x)BNLT-xBT Ceramics System
- 3 October 2007
- journal article
- Published by Taylor & Francis in Ferroelectrics
- Vol. 358 (1) , 129-133
Abstract
The preparation of Lead-free piezoelectric ceramics of lanthanum doped bismuth sodium tinanate (Bi 0.487 Na 0.487 La 0.017 TiO 3 : BNLT) and barium titanate (BaTiO 3 : BT) have been carried out in the system of (1−x)BNLT-xBT where x = 0, 0.2, 0.4, 0.8 and 1.0. The BNLT and BT powders were produced separately using conventional method and they were then mixed by following above ratios. Physical, dielectric and piezoelectric properties were also observed. The optimum sintering temperatures of ceramics are in the range of 1100°C to 1150°C with a soaking time for 2 hours. The optimum conditions in terms of microstructure, physical, dielectric and piezoelectric properties were found in the (1−x)BNLT-xBT ceramic with x = 0.2.Keywords
This publication has 5 references indexed in Scilit:
- Piezoelectric and ferroelectric properties of lead-free [Bi1−y(Na1−x−yLix)]0.5BayTiO3 ceramicsJournal of the European Ceramic Society, 2006
- Some effects of different additives on dielectric and piezoelectric properties of (Bi1/2Na1/2)TiO3–BaTiO3 morphotropic-phase-boundary compositionMaterials Letters, 2004
- Large Piezoelectric Constant and High Curie Temperature of Lead-Free Piezoelectric Ceramic Ternary System Based on Bismuth Sodium Titanate-Bismuth Potassium Titanate-Barium Titanate near the Morphotropic Phase BoundaryJapanese Journal of Applied Physics, 2003
- (Reactive) Templated Grain Growth of Textured Sodium Bismuth Titanate (Na1/2Bi1/2TiO3-BaTiO3) Ceramics—II Dielectric and Piezoelectric PropertiesJournal of Electroceramics, 2003
- Processing and Electromechanical Properties of (Bi0.5Na0.5)(1−1.5x)LaxTiO3CeramicsJournal of the American Ceramic Society, 1997