Biaxial Strain Engineering of Thermoelectric Properties of Bi2Te3: A First-Principles Study

Authors:

Abstract
We present a systematic first-principles investigation of the effect of biaxial in-plane strain on the structural, electronic, and thermoelectric properties of bismuth telluride (Bi2Te3) using the Full-Potential Augmented Plane Wave plus local orbitals (FP-APW+lo) method implemented in WIEN2k [15]. The exchange-correlation potential is described by the Perdew-Burke-Ernzerhof (PBE) generalized gradient approximation [16] supplemented by the modified Becke-Johnson (mBJ) potential [17] with spin-orbit coupling (SOC). Five biaxial in-plane strains of ε = −2%, −1%, 0%, +1%, and +2% are systematically applied. The calculated band gap at zero strain is 0.123 eV, in excellent agreement with the experimental value of 0.13–0.17 eV [6,25], demonstrating the advantage of the mBJ+SOC approach over conventional PBE+SOC [14]. The band gap varies linearly with strain at a rate of −8 meV/%, increasing under compressive strain and decreasing under tensile strain. Thermoelectric transport properties are computed using BoltzTraP2 [19] within the constant relaxation time approximation. Under −2% compressive strain, the Seebeck coefficient reaches 343 μV/K (p-type) and 216 μV/K (n-type) at n = 1019 cm−3 and T = 300 K. The figure of merit ZT is maximized at ε = −2%, yielding ZTₚ = 0.474 (+31%) and ZTₙ = 0.570 (+7%) over the unstrained case at optimal carrier concentrations of ~5×1018 and ~7×1018 cm−3, respectively.

This publication has 24 references indexed in Scilit: