High‐temperature stabilization of polypropylene using hindered phenol–thioester stabilizer combinations, Part 2: Optimization and efficacy via encapsulation with silicate fillers
Authors:
- 2 February 2021
- journal article
- research article
- Published by Wiley in Journal of Vinyl and Additive Technology
- Vol. 27 (2) , 389-409
Abstract
The thermal degradation of unstabilized polypropylene has been investigated under long‐term thermal aging at 150°C, with additive concentration studies on combinations of an established hindered phenolic antioxidant (pentaerythritol tetrakis (3‐(3,5‐di‐tert‐butyl‐4‐hydroxyphenyl) propionate) [S1010] and two popular thioesters (distearyl‐3,3′‐thiodipropionate [DSTDP] and didodecyl‐3,3′‐thiodipropionate [DLTDP]) using melt flow rate (MFR), carbonyl index (Fourier transform spectroscopy [FTIR]) and differential scanning calorimetry (DSC) (oxidation induction time [OIT]) and ultimate embrittlement time (fracture) on injection‐molded test pieces. It was found in part 1 that 20:80 phenol:thioester ratios provided the best long‐term thermal stability (LTTS). Part 2 investigates potential improvements in stabilization, involving the use of controlled release systems in which the stabilizers are melt blended in the PP together with high surface area inorganic substrates. Here, a calcined gel silica SD3128 and two layered silicates Rockwood Additives Fulcat® 800 and Laponite® B were incorporated into the polymer formulations in order to limit stabilizer mobility at 6000 ppm through potential surface adsorption and subsequent controlled release. Additional hindered amine light stabilizers were also added as long‐term heat stabilizers and to act as displacing agents that promote controlled release via competitive adsorption on processing due to the strongly adsorbing amine functionalities. In some instances, the LTTS showed improvement. Flow micro calorimetry was used to investigate the stabilizer–substrate interactions. It was found that as a result of its small pore structure, Laponite B could only adsorb smaller molecules such as that of DLTDP while Fulcat® 800 was a more strongly adsorbing substrate with larger pores able to accommodate even the largest of the hindered amine light stabilizer (HALS) molecules. The gel silica SD3128 had overall the most adsorbing ability with each of these characteristics supporting the aging data studied in parallel. The data are discussed in relation to the long‐term stabilization of polypropylene in high‐temperature applications such as under the bonnet of automobiles where minimizing stabilizer losses and maximizing synergy are important.Keywords
This publication has 26 references indexed in Scilit:
- Kinetic modelling of stabilization coupled with stabilizer loss by evaporation. Case of dithioester stabilized polyethylenePolymer Degradation and Stability, 2009
- Synergism between polymer antioxidants—kinetic modellingPolymer Degradation and Stability, 2003
- Stabilisation of LDPE cross-linked in the presence of peroxidesII. FTIR study of chemical changes taking place in the LDPE–dicumyl peroxide–Irganox 1081 systemPolymer Degradation and Stability, 2000
- Plastics Additives1998
- A New Kinetic Model for Polypropylene Thermal Oxidation at Moderate TemperaturesMacromolecules, 1997
- Antioxidant action of organic sulphites—I. Esters of sulphurous acid as secondary antioxidantsPolymer Degradation and Stability, 1997
- Effect of Stabilization of Polypropylene during Processing and Its Influence on Long-Term Behavior under Thermal Stress1996
- Studies on polymer stabilizers: Part II. A new concept of a synergistic mechanism between phenolic and thiopropionate type antioxidantsPolymer Degradation and Stability, 1992
- Environmental degradation of polypropylenePolymer Degradation and Stability, 1988
- The Role of Certain Organic Sulfur Compounds as Preventive Antioxidants. II. Activity as Peroxide Decomposers and Effect of BasesRubber Chemistry and Technology, 1976