Effect of powder bed preheating on distortion and mechanical properties in high speed selective laser melting
Authors:
Open Access
- 1 October 2019
- conference paper
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 655 (1) , 012026
Abstract
Selective Laser Melting (SLM) is known to cause residual stresses due to the inherent large thermal gradients from high heating and cooling rates during manufacturing. The residual stresses tend to induce distortion, delamination of parts from the base plate as well as cracking because they reduce the threshold flaw size required for crack initiation. These challenges form a barrier to the use of this additive manufacturing method for structural applications for the aerospace industry where high part integrity is a critical requirement. The aim of the study was to evaluate the degree of distortion and crack growth resistance during increasing monotonic loading and cyclic loading of As-built Ti6Al4V parts produced on the Aeroswift high speed SLM process preheated at 200°C. The monotonic loading results are comparable to those of commercial SLM systems but are lower when compared conventional manufacturing methods. The crack growth resistance of the As-built specimen is lower than that of heat treated specimen. Distortion at this preheating temperature is evident at from 12cm away from the base of the cantilever and spreads to height of 3.2mm.Keywords
This publication has 15 references indexed in Scilit:
- Reducing residual stress by selective large-area diode surface heating during laser powder bed fusion additive manufacturingAdditive Manufacturing, 2019
- Improvement of the bridge curvature method to assess residual stresses in selective laser meltingAdditive Manufacturing, 2018
- Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti-6Al-4V: A reviewInternational Journal of Machine Tools and Manufacture, 2018
- In-situ residual stress reduction, martensitic decomposition and mechanical properties enhancement through high temperature powder bed pre-heating of Selective Laser Melted Ti6Al4VMaterials Science and Engineering: A, 2017
- An improved prediction of residual stresses and distortion in additive manufacturingComputational Materials Science, 2017
- Metal Additive Manufacturing: A Review of Mechanical PropertiesAnnual Review of Materials Research, 2016
- A study on the residual stress during selective laser melting (SLM) of metallic powderThe International Journal of Advanced Manufacturing Technology, 2016
- Crack propagation and fracture toughness of Ti6Al4V alloy produced by selective laser meltingAdditive Manufacturing, 2015
- On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performanceInternational Journal of Fatigue, 2013
- Residual stresses in selective laser sintering and selective laser meltingRapid Prototyping Journal, 2006