Study of the deep drawing behavior and crystallographic texture of AA 3104-H19 aluminum alloy sheets
Authors:
- 13 May 2016
- journal article
- research article
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
- Vol. 230 (3) , 748-759
Abstract
The aluminum alloy 3104, H19 temper, is commonly used in the production of two-piece beverage cans. The objective of the present study is to compare three different rolled sheets of this alloy. All three of them are routinely used in production lines dedicated to can manufacturing. The yield strength for all three was found around 265 MPa, the ultimate tensile strength 281 MPa, and the average elongation 4.19%. The strain hardening exponent (n) was similar for all three sheets, averaging 0.078. The plastic strain ratios for planar anisotropy (ΔR) and for normal anisotropy ( ) were found to be near zero and 0.4, respectively. Values of ΔR near zero indicate there is no earing tendency. The crystallographic texture analysis yielded four dominating components: Brass ({110}) and Copper ({112}), which are typical of strain hardened aluminum, Cube ({001}), usually associated with recrystallization, and Goss ({110}). Such a texture would be conducive to balanced earing. The metallographic images for all three sheets were alike, with constituents not homogeneously distributed and with similar size and chemical compositions in addition to dispersoids finely spread throughout the aluminum matrix. The Erichsen tests also showed alike results with an average of 4.6 mm before failure.
Keywords
This publication has 11 references indexed in Scilit:
- On the Work-Hardening of AA 3104-H19 Aluminum AlloyJournal of Materials Engineering and Performance, 2012
- Control of texture and earing in aluminium alloy AA 3105 sheet for packaging applicationsMaterials Science and Engineering: A, 2012
- Texture-based design of a convoluted cut-edge for earing-free beverage cansJournal of Materials Processing Technology, 2011
- Impact of die wear and punch surface textures on aluminium can wallWear, 2009
- Analysis of the manufacturing process of beverage cans using aluminum alloyJournal of Materials Processing Technology, 2008
- Polycrystal-plasticity simulation of six and eight ears in deep-drawn aluminum cupsMaterials Science and Engineering: A, 2007
- Energetic analysis of tube drawing processes with fixed plug by upper bound methodJournal of Materials Processing Technology, 2006
- Influence of surface topography on the frictional characteristics of 3104 aluminum alloy sheetWear, 1996
- Correlation between the preferred grain orientation and the deep-drawing behavior of AA 3104 and AA 5052 aluminum alloy sheetsScripta Metallurgica et Materialia, 1994
- The effect of cold working and annealing practice on earing in 3104 Al alloy sheetMaterials Characterization, 1993