Sintering of High‐Purity Magnesia

Authors:

Abstract
The effect of calcining temperatures on the sinter ability of high‐purity magnesia powders was investigated. A marked decrease in the density of sintered (fired) compacts occurred when petro‐graphically identifiable periclase was formed in calcining. By employing proper heat‐treatment in calcining the powder, ceramic bodies with zero apparent porosities were obtained at sintering temperatures as low as 1650°C. It is suggested that proper calcinations might also facilitate the preparation of dense ceramics of other oxides.