Novel Rubbers from Cationic Copolymerization of Soybean Oils and Dicyclopentadiene. 1. Synthesis and Characterization

Authors:

Abstract
Novel thermosetting copolymers, ranging from tough and ductile to very soft rubbers, have been prepared by the cationic copolymerization of regular (SOY) and 100% conjugated soybean oils (C100SOY) with dicyclopentadiene (DCP) catalyzed by Norway fish oil (NFO)-modified and SOY- and C100SOY-diluted boron trifluoride diethyl etherate (BFE). The gelation time of the reactions varies from 4 to 991 min at 110 °C. The yields of the bulk copolymers are essentially quantitative, while the yields of the cross-linked copolymers remaining after Soxhlet extraction with methylene chloride range from 69% to 88%, depending on the monomer stoichiometry and the catalyst used. 1H NMR spectroscopy and Soxhlet extraction data indicate that these copolymers consist of a cross-linked soybean oil−DCP network plasticized by certain amounts of methylene chloride-soluble linear or less cross-linked soybean oil−DCP copolymers, unreacted oil, and some low molecular weight hydrolyzed oil. The molecular weights of these soluble fractions are in the range from 400 to 10 000 g/mol based on polystyrene standards. The bulk copolymers have glass transition temperatures ranging from −22.6 to 56.6 °C, while their tan δ peak values range from 0.7 to 1.2. Thermogravimetric analysis (TGA) indicates that these soybean oil−DCP copolymers are thermally stable below 200 °C, with 10% and 50% weight loss temperatures ranging from 280 to 372 °C and 470−554 °C, respectively. These properties suggest that these biobased thermosets may prove useful alternatives to current petroleum-based plastics and find widespread utility.

This publication has 8 references indexed in Scilit: