Silicon Carbide Powder Synthesis from Silicon Monoxide and Methane
Authors:
- 1 March 1997
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 80 (3) , 757-760
Abstract
SiC was synthesized via the gas‐phase reaction between SiO and CH4 at 1500° and 1560°C in a tubular flow reactor. SiO vapor was generated from equimolar powder mixtures of Si and SiO2 in the reactor while CH4 was externally supplied. Products of different morphologies were collected at different longitudinal locations: whiskers, crystal aggregates, scale, and powder. The total yield of SiC, based on the amount of SiO generated, reached as high as 99%, of which 25–46% by mass was fine powder with sizes ranging from 60 to 300 nm.Keywords
This publication has 18 references indexed in Scilit:
- Induction plasma synthesis of ultrafine SiC powders from silicon and CH4Journal of Materials Science, 1995
- Carbon Dioxide laser Synthesis of Ultrafine Silicon Carbide Powders from DiethoxydimethylsilaneJournal of the American Ceramic Society, 1994
- Preparation of monodispersed spherical silicon carbide by the sol-gel methodJournal of Materials Science, 1993
- Kinetics of carbothermal reduction synthesis of beta silicon carbideAIChE Journal, 1993
- Synthesis of ultra-fine SiC powders in a d.c. plasma reactorJournal of Materials Science, 1993
- Low-temperature synthesis of sinterable SiC powders by carbothermic reduction of colloidal SiO2Journal of Materials Science, 1992
- Production of Fine, High‐Purity Beta Silicon Carbide PowdersJournal of the American Ceramic Society, 1992
- Synthesis of Monodispersed Spherical β‐Silicon Carbide Powder by a Sol‐Gel ProcessJournal of the American Ceramic Society, 1990
- Laser synthesis and crystallographic characterization of ultrafine SiC powdersJournal of Materials Research, 1990
- Laser Synthesis of Silicon Carbide Powders from Silane and Hydrocarbon MixturesAdvanced Ceramic Materials, 1988