Wire-shaped austenite (γ) and γ+lath martensite (α'T) duplex phase alloys of Fe-Ni-Si-C and Fe-Ni-Cr-Si-C systems exhibiting high strengths and large elongation have been produced by melt spinning in rotating water. The wire formation is limited to the compositions above about 6 at% Ni, 4 to 13 at% Si and 2 to 8 at% C /or the γ structure and above about 4 at% Ni, 2 to 10 at% Si and below 6 at% C for the γ+α'L structure. The wires have a circular section with a diameter in the range of 80 to 140μm. The average grain size of γ phase is as small as 1.0 to 1.5μm. The 0.2% proof strength (σy) and tensile strength (σf) of γ structure wires increase from 310 to 650MPa and from 490 to 960MPa, respectively, with the amounts of Si, C and/or Cr, while elongation (εp) decreases from 24 to 9%. The σy and σf of the γ+α'L wires exhibit an compositional dependence inverse to that for the γ wires. With decreasing Si and C contents, the σy and σf increase from 360 to 1100MPa and from 900 to 1600MPa, respectively, and the εp decreases from 18 to 0.5%. Cold drawing causes significant increases in σy up to 2750MPa and σf to 3000MPa for Fe-20Ni-12Si-2C wire drawn about 90% reduction in area. Achievement of the high strengths is attributed to work-hardenability of γ and α' phases and formation of strain-induced fibrous α' phase.