In Vitro Behavior of Silica‐Based Xerogels Intended as Controlled Release Carriers
Authors:
- 1 April 1999
- journal article
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 82 (4) , 969-976
Abstract
We report on the in vitro behavior of room‐temperature‐prepared xerogels upon immersion in typical physiologic solutions. The effect of various parameters was studied: xerogel composition and particle size; solution composition; and immersion protocol. Three xerogel compositions were tested: a silica xerogel (S100); a Vancomycin–silica xerogel composite (S100V); and a calcium‐ and phosphorus‐containing silica xerogel (S70). The immersion was per‐formed integrally (i.e., without solution exchange) or dif‐ferentially (i.e., with solution exchange) to model the continuous flow of body fluids past implant surfaces. Four different solutions were used: tris(hydroxymethyl)amino‐methane hydrochloric acid buffer solution plus electrolytes (TE); TE supplemented with 3% H 2 O 2 ; TE supplemented with 10% serum; and serum. Carbonated hydroxyapatite formed on all xerogels. The reaction was faster on S70 than on S100. The silica network fully dissolved for all xerogels in the differential experiment. S70 particles transformed to calcium‐ and phosphorus‐containing “shells” upon differ‐ential immersion. The presence of H2 O2 and serum proteins in the immersion solution slowed down the silicon dissolu‐tion of both xerogels. Xerogel dissolution was associated with decreased BET surface area and increased mean pore size. The data showed a linear relationship between the dissolution rate and the time‐dependent surface area. Re‐gardless of this relationship, our data also suggested that the rate‐limiting step of the dissolution during integral im‐mersion was the diffusion of the dissolved species to the bulk solution.Keywords
This publication has 21 references indexed in Scilit:
- In vitro release kinetics of biologically active transforming growth factor-β1 from a novel porous glass carrierBiomaterials, 1997
- Glass Wool–H2O2/CoCl2 test system for in vitro evaluation of biodegradative stress cracking in polyurethane elastomersJournal of Biomedical Materials Research, 1995
- Stimulation of bone healing by transforming growth factor‐beta1 released from polymeric or ceramic implantsJournal of Applied Biomaterials, 1994
- Effect of Treatment of Reactive Aggregate by H 2 O 2 on the Alkali‐Silica ReactionJournal of the American Ceramic Society, 1994
- Structural Evolution of Alkoxide Silica Gels to Glass: Effect of Catalyst pHJournal of the American Ceramic Society, 1993
- Treatment of experimental osteomyelitis with antibiotic‐impregnated bone graft substituteJournal of Orthopaedic Research, 1993
- Variations between biomer lots. 2: The effect of differences between lots on in vitro enzymatic and oxidative degradation of a commercial polyurethaneJournal of Biomedical Materials Research, 1993
- Antibiotic Prophylaxis in Orthopedic SurgeryClinical Infectious Diseases, 1991
- Titanium-hydrogen peroxide interaction: model studies of the influence of the inflammatory response on titanium implantsBiomaterials, 1989
- Aging of Amorphous Silica in Salt Water Solutions1982