High-frequency permeability of (Fe, Co, Ni)62Nb8B30 amorphous alloys with a wide supercooled liquid region

Authors:

Abstract
The increase in B content to 30 at. % for Fe–Co–Ni–Nb–B amorphous alloys caused an extension of a supercooled liquid region before crystallization, and a wide supercooled liquid region greater than 80 K was obtained in a wide composition range of 5–42 at. % Co and 0–10 at. % Ni for Fe62−x−yCoxNiyNb8B30 amorphous alloys. High B-containing amorphous alloys with low Ni content below 10 at. % have high electrical resistivity above 230 μΩ cm and exhibit good soft magnetic properties, i.e., a low coercive force of 2 A/m, low saturated magnetostriction of 2–7×10−6, and high permeability of 21 000–29 300 at 1 kHz and 5000–7500 at 1 MHz. The high-frequency permeability characteristics at 1 MHz are much better than those for any kind of soft magnetic materials, and have been presumed to result from the decrease in eddy current loss caused by the increase in electrical resistivity. The synthesis of the Fe–Co–Nb–B amorphous alloys exhibiting a wide supercooled liquid region greater than 80 K and high-frequency permeability of 7500 at 1 MHz is promising for future development as a type of soft magnetic material.

This publication has 17 references indexed in Scilit: