Design of a non‐shrinking silica fume high‐performance concrete with recycled ceramic tile aggregate
- 3 December 2022
- journal article
- research article
- Published by Wiley in Structural Concrete
- Vol. 24 (3) , 3425-3442
Abstract
Internal curing (IC) process introduced via a water‐entraining agent using lightweight and porous aggregate has become an essential component in designing high and ultra‐high‐performance concrete (HPC/UHPC). This paper presents experimental results demonstrating the effectiveness of using recycled ceramic tile aggregates (RCTA) derived from waste ceramic tiles as an IC agent for high‐performance structural elements. Previous studies by the author have confirmed the efficiency of both the pre‐saturated recycled porous ceramic coarse aggregate (RPCA) as an IC and shrinkage compensating agents in mitigating autogenous shrinkage and the induced internal self‐stress in HPC mixtures. The main objective of this study is to investigate the effect of two different curing systems (internal curing using the waste ceramic aggregate combined with shrinkage compensating agents) on silica fume (SF) HPC behavior. The shrinkage compensating agents include a combination of shrinkage‐reducing agent (R) and expansive additive (E). The influence of this combined ternary curing system on the mechanical properties, including compressive, flexural, and splitting tensile strengths, modulus of elasticity, autogenous shrinkage, and internal self‐induced tensile stress, were investigated. The obtained results indicate a substantial reduction in the autogenous shrinkage strains magnitude and, consequently, the internal self‐induced tensile stress in the HPC mixtures designed with these two curing systems. It was also found that this combination of the two curing systems resulting in a hybrid curing system, performs much better than the single incorporation of shrinkage‐compensating agents. Besides, a long‐term strengths improvement was recorded for mixtures designed with the RPCA. Incorporating recycled aggregate in the design and production of HPC could further promote concrete sustainability by reducing the amount of virgin extracted non‐renewable minerals, reducing the energy required to extract and process natural aggregates and the CO2 generated, and also reducing solid waste materials disposal.Keywords
This publication has 45 references indexed in Scilit:
- Utilization of ceramic waste as fine aggregate within Portland cement and fly ash concretesCement and Concrete Composites, 2010
- Use of porous ceramic waste aggregates for internal curing of high-performance concreteCement and Concrete Research, 2009
- Mechanical properties of brick aggregate concreteConstruction and Building Materials, 2009
- Behaviour of cementitious mortars containing different kinds of recycled aggregateConstruction and Building Materials, 2009
- Shrinkage crack reducing effects in actual floor slabs by combining SRA and expansive agents in concrete2008
- Structural concrete with incorporation of coarse recycled concrete and ceramic aggregates: durability performanceMaterials and Structures, 2008
- Recycled aggregate concrete as structural materialMaterials and Structures, 2006
- Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregatesCement and Concrete Research, 2001
- Shrinkage-reducing admixtures and early-age desiccation in cement pastes and mortarsCement and Concrete Research, 2001
- Properties of high-performance concrete containing shrinkage-reducing admixtureCement and Concrete Research, 1997