Characteristics of Solidified Products Containing Radioactive Molten Salt Waste
Authors:
- 3 October 2007
- journal article
- research article
- Published by American Chemical Society (ACS) in Environmental Science & Technology
- Vol. 41 (21) , 7536-7542
Abstract
The molten salt waste from a pyroprocess to recover uranium and transuranic elements is one of the problematic radioactive wastes to be solidified into a durable wasteform for its final disposal. By using a novel method, named as the GRSS (gel-route stabilization/solidification) method, a molten salt waste was treated to produce a unique wasteform. A borosilicate glass as a chemical binder dissolves the silicate compounds in the gel products to produce one amorphous phase while most of the phosphates are encapsulated by the vitrified phase. Also, Cs in the gel product is preferentially situated in the silicate phase, and it is vitrified into a glassy phase after a heat treatment. The Sr-containing phase is mainly phosphate compounds and encapsulated by the glassy phase. These phenomena could be identified by the static and dynamic leaching test that revealed a high leach resistance of radionuclides. The leach rates were about 10-3∼10-2g/m2·day for Cs and 10-4∼10-3g/m2·day for Sr, and the leached fractions of them were predicted to be 0.89% and 0.39% at 900 days, respectively. This paper describes the characteristics of a unique wasteform containing a molten salt waste and provides important information on a newly developed immobilization technology for salt wastes, the GRSS method.Keywords
This publication has 9 references indexed in Scilit:
- Immobilization of fission products arising from pyrometallurgical reprocessing in chloride mediaJournal of Nuclear Materials, 2005
- Candidate wasteforms for the immobilization of chloride-containing radioactive wasteJournal of Non-Crystalline Solids, 2004
- Treatment of molten salt wastes by phosphate precipitation: removal of fission product elements after pyrochemical reprocessing of spent nuclear fuels in chloride meltsJournal of Nuclear Materials, 2003
- Characterization of cesium containing glass-bonded ceramic waste formsMicroporous and Mesoporous Materials, 2003
- The precision of product consistency tests conducted with a glass-bonded ceramic waste formJournal of Nuclear Materials, 2002
- Immobilization of CsCl and SrF2 in iron phosphate glassWaste Management, 2000
- On the reactive occlusion of the (uranium trichloride + lithium chloride + potassium chloride) eutectic salt in zeolite 4AJournal of Nuclear Materials, 2000
- Immobilization of spent nuclear fuel in iron phosphate glassJournal of Nuclear Materials, 1999
- Conversion Reactions of Metal Chlorides into Oxides with Boric Acid Applicability to the Vitrification of Molten Salt Wastes Generated in Pyro-reprocessing ProcessJournal of Nuclear Science and Technology, 1995