UV Irradiation Effects on Chemical Vapor Deposition of SiO2

Authors:
  • JTJun-Ichi Takahashi
    Jun-Ichi Takahashi
  • MTMichiharu Tabe
    Michiharu Tabe

Abstract
Silica (SiO2) films have been deposited from a SiH4+O2+Ar system under 1849 Å irradiation by a low pressure Hg lamp without using Hg photosensitization. The oxygen partial pressure (P O2 ) dependence of the deposition rate has been measured in order to investigate the effects of 1849 Å irradiation. In a low P O2 region, it is found that the increase-maximum-decrease profile due to surface reaction in thermal CVD is modified under 1849 Å irradiation. The modification of the curve profile caused by 1849 Å irradiation is due to photodesorption of adsorbed oxygen molecules from the surface. In a high P O2 region, SiO2 deposition is observed under 1849 Å irradiation, while SiO2 is not deposited in thermal CVD. In this region the gas phase reaction is predominant.

This publication has 7 references indexed in Scilit: